Repairing Cast Iron casting defects with colour match, Oil soaked cast Iron parts, Buffer layer in joining & cladding of grey & Nodular cast Iron.
Most suitable for repairing all types of cast iron. Nickle free deposit provides colour match to cast Iron & gets oxidized. Can be used on thin & thick sections of Cast Iron. Suitable for joining Cast Iron to steel. Performs extraordinary on contaminated or oxidized surfaces.
Make a V groove using Excel Gouge after drilling holes at the end of the cracks. Use AC or DC reverse polarity. Use medium arc to seal the contaminated surfaces. Avoid weaving. Do deposit 5-10 Cms bead, avoid continuous welding, leave a gap & come back on the position to complete the job. Remove slag after every pass.
SIZE (mm) | AMPERAGE |
3.15 | 105 – 125 |
4.00 | 130-150 |
1. Hardness: 40-45 HRC