Cast Iron Pulleys, Gears, Sliding table machines, Water Jacket leakage, casting defects.
Excellent for thin walled Cast Iron castings. Excellent of building up missing section, cladding, filling holes, repairing broken , cracked & fabricated components of cast Iron to steel. Excellent out of position welding.
Gouge out crack with “Excel Gouge” Grind it, clean surface impurities mechanically, preheat up to 2000C. Use short to medium arc at minimum amperage. Peen the weld to stress relieved. Skip weld to avoid the heat concentration. For more in depth of procedure contact Excel Craft welding expert.
SIZE (mm) | AMPERAGE |
400 | 80 – 100 |
3.15 | 55 – 80 |
2.50 | 55 - 70 |
2.00 | 35 - 45 |
1. Tensile Strength > 50,000 psi